Sol–Gel-Encapsulated Biofilms on Biochar Effectively Degrade PCBs and Extend Biodegradation Activity under Environmentally Relevant Conditions
Journal article   Open access   Peer reviewed

Sol–Gel-Encapsulated Biofilms on Biochar Effectively Degrade PCBs and Extend Biodegradation Activity under Environmentally Relevant Conditions

Qin Dong, Weilun Zhao, Andres Martinez, Rachel F. Marek, Keri C. Hornbuckle, Xueshu Li, Hans-Joachim Lehmler, Gregory H. LeFevre and Timothy E. Mattes
Environmental science & technology, Vol.60(40), pp.28886-28898
09/25/2026
DOI: 10.1021/acs.est.6c02869
PMCID: PMC13674062
PMID: 42915955
url
https://doi.org/10.1021/acs.est.6c02869View
Published (Version of record) Open Access

Abstract

Attaching aerobic, PCB-degrading cells to carbon-based sorbent materials prior to sediment application is a feasible approach for bioaugmenting contaminated sediments to improve remediation strategies. Furthermore, encapsulation of attached cells with a novel, tailored sol–gel material can protect biofilms from unfavorable environmental conditions that interfere with biofilm stability and create stress that threatens long-term biofilm viability. We systematically evaluated biodegradation and sorption of three PCB congeners (PCBs 4, 18, and 52), quantified biphenyl dioxygenase gene (bphA) abundance and expression, and characterized sol–gel and biofilm integrity of sol–gel-coated PCB-degrading biofilms on black carbon over 45 days under environmentally relevant conditions. Sol–gel coatings did not significantly inhibit PCB sorption to the black carbon, and sol–gel-coated biofilms achieved 72–92% PCB removal within 45 days, comparable to uncoated biofilms (>91%). Although PCB biodegradation rates in uncoated biofilms were >5-fold higher than sol–gel-coated biofilms, sol–gel-coated biofilms maintained >2-fold higher bphA expression levels than uncoated biofilms after 45 days of treatment. Lower temperature (10 °C) decreased PCB biodegradation extent regardless of sol–gel coating but significantly increased (10-fold higher) bphA expression levels in sol–gel-coated biofilms. Salinity (20 g/L) negatively impacted bphA expression levels (>13-fold lower after 45 days) for all treatments. Our novel sol–gel design demonstrates dual benefits: to sorb PCBs from the environment to biofilms and provide carbon sources for PCB cometabolism, thereby protecting and supporting biofilms for potential extended activity in future field applications.
sol-gel encapsulation PCB biodegradation environmental condition impacts